ISO 4628-3 coated-surface rusting-area reference (Ri 0–Ri 5), used with ISO 9223 environmental corrosivity
Taiwan atmospheric corrosion station dataSurface is intact with no visible signs of corrosion. Metal retains original luster with no rust or oxidation.
Very few corrosion spots appear on the surface, typically early oxidation spots or slight discoloration; the reference area is approximately 0.05%.
Visible corrosion spots appear, with a reference rusted area of approximately 0.5%. Rust spreading is visible but the substrate is not severely attacked.
The reference rusted area is approximately 1%, with patches of rust; coating condition and substrate damage still require separate site assessment.
The reference rusted area is approximately 8%, with larger rusted patches; coating loss, pitting and structural consequences require site inspection.
The reference rusted area is approximately 40%–50%, representing the most severe visual rusting class; shutdown and repair decisions require a qualified engineer's site assessment.
| Grade | Affected Area | vs. prior class | Risk | Action |
|---|---|---|---|---|
| Ri 0 | 0% | — | Very Low | Annual inspection |
| Ri 1 | 0.05% | 起始 | Low | Semi-annual inspection |
| Ri 2 | 0.5% | ×10 | Medium-Low | Local rust removal |
| Ri 3 | 1% | ×2 | Medium | Full rust removal & recoating |
| Ri 4 | 8% | ×8 | High | Emergency repair |
| Ri 5 | 40%–50% | ×5–×6 | Extreme | Immediate site assessment |
ISO 4628-3 compares coating rusting against pictorial standards rather than equal area increments. The Ri 1–Ri 4 reference areas are 0.05%, 0.5%, 1% and 8%.
This scale is particularly sensitive to early rusting, helping teams plan protection while affected area remains small. Ri 5 has a visual reference area of approximately 40%–50%. Area class alone does not determine substrate loss or structural damage; separate measurement and engineering judgement are required.
* Ri classification follows ISO 4628-3 pictorial standards for coating rusting. ISO 8501-1 covers uncoated steel rust grades and cleanliness; ISO 9223 covers atmospheric corrosivity. Actual assessment should be confirmed by a qualified engineer on-site.
Use alongside Ri 0–Ri 5 image grading results with environmental data to improve maintenance recommendation accuracy.
| Grade | Corrosivity | Carbon Steel Annual Rate | Typical Locations |
|---|---|---|---|
| C1 | Very Low | < 1.3 μm/year | Indoor dry environments |
| C2 | Low | 1.3–25 μm/year | Suburban, general indoor |
| C3 | Medium | 25–50 μm/year | Urban, light industrial, humid outdoor |
| C4 | High | 50–80 μm/year | Coastal 1–10km, port areas, industrial zones |
| C5 | Very High | 80–200 μm/year | High-salt coastal areas |
| CX | Extreme | 200–700 μm/year | Extreme marine environments (splash zone, offshore) |
| Standard | Name | Purpose |
|---|---|---|
| ISO 8501-1:2007 | Visual assessment of surface cleanliness | Original rust grades A–D and cleaning grades Sa 1–3, St 2–3 |
| ISO 9223:2012 | Atmospheric corrosivity classification | Environmental corrosivity (C1–CX) |
| ISO 9224 | Corrosion rate classification | Quantify corrosion rates |
| NACE SP0169:2013 | External corrosion control | Pipeline external corrosion & area grading |
| ISO 4628-3:2016 | Assessment of degree of rusting | Ri 0–Ri 5 pictorial rusted-area reference |
| CNS 13401 (ISO 9223) | Taiwan national standard | Local standard aligned with ISO 9223 |