This document serves as the internal reference for AI image recognition grading (L0–L5) and international standards alignment, for engineering integration, report writing, and client communication.
Judgment basis: AI grades solely based on visual corrosion appearance in photos (area, depth, color, morphology)
Not considered: Environmental factors (temperature, humidity, salinity, service life)
Analogy framework: Think of equipment as a patient — L0 healthy → L5 organ failure
| AI Grade | Patient Analogy | Visual Characteristics | ISO 8501-1 Correspondence | NACE Area Grade | Recommended Action |
|---|---|---|---|---|---|
| L0 | Perfectly Healthy | Smooth intact surface, no rust spots, coating/plating intact | Sa 3 / St 3 (Near-perfect cleanliness) | NACE 0 | Regular visual inspection, maintain current state |
| L1 | Mild Cold | Very minor spot rust or surface oxidation discoloration, substrate not damaged | Grade A (Mild mill scale) | NACE 1 (<10% area) | Regular cleaning, protective coating reinforcement |
| L2 | Skin Inflammation | Expanding rust area, visible reddish-brown rust spots, surface roughening | Grade B–C (Partial mill scale spalling) | NACE 2 (10–40% area) | Localized rust removal + primer recoating |
| L3 | Dermis Damage | Rust penetrating protective layer, rust streaks, localized pitting, structural damage beginning | Grade C–D (Large-area mill scale spalling) | NACE 3 (40–70% area) | Full sandblasting + anti-corrosion coating system |
| L4 | Organ Damage | Large-area deep corrosion, significant pitting, lamellar spalling, structural strength declining | Grade D (Severe mill scale and pitting) | NACE 4 (70–90% area) | Emergency shutdown assessment + structural reinforcement or partial replacement |
| L5 | Organ Failure | Perforation/fracture risk, corrosion through cross-section, equipment at service limit | Beyond ISO 8501-1 assessment scope (on-site engineer evaluation required) | NACE 5 (>90% area) | Immediate decommission, full structural assessment and replacement |
| Grade | Corrosivity | Corrosion Rate (Steel) | Typical Environment |
|---|---|---|---|
| C1 | Very Low | <1.3 μm/year | Dry indoor environments (offices, residences) |
| C2 | Low | 1.3–25 μm/year | Low-pollution rural areas |
| C3 | Medium | 25–50 μm/year | Urban, light industrial areas |
| C4 | High | 50–80 μm/year | Industrial zones, coastal cities |
| C5 | Very High | 80–200 μm/year | Taiwan coastal high-salinity zones |
| CX | Extreme | 200–700 μm/year | Extreme marine environments (splash zones, offshore facilities) |
| Standard | Name | Purpose |
|---|---|---|
| ISO 8501-1:2007 | Visual assessment of surface cleanliness before painting | Rust grade determination (Sa 1–3, St 2–3) |
| ISO 9223:2012 | Atmospheric corrosivity classification | Environmental corrosivity (C1–CX) |
| ISO 9224 | Corrosion rate classification of metallic materials | Corrosion rate quantification |
| NACE SP0169:2013 | External corrosion control specification | Pipeline external corrosion control and area grading |
| ISO 4628 | Coating degradation assessment | Rust, blistering, flaking grade assessment |
| CNS 13401 (ISO 9223) | Taiwan national standard | Local standard aligned with ISO 9223 |